r/18650masterrace • u/Critical-Truth8409 • 12h ago
Help me identify oily residue on spot welds when assembling pack
Hello everyone,
I am currently assembling a 10s4p molicel p42a pack.
I've assembled them using a kweld with the following parameters :
sandwich method : 0.1 mm stainless steel on top of 0.2 mm copper (pre-glued stainless steel pads on top of the copper, see pictures below)
three 85 J pulses on each cell pole from a lead-acid battery power supply
I did many tests on 18650 cells using 85 J pulses and it went fine with no sign of puncturing after pulling the welds off.
So far the pack looks like this :


A week later, I come back to finish building it and I find some brownish-orange oily spots on some negative poles of like ~12 cells, please see the picture below :
Before cleaning (with IPA) :


After cleaning :

There is no strange smell that would indicate electrolyte and, after cleaning, the welds look like the others.
Also, no more liquid appears and the weld stays dry.
My hypothesis are the following :
it is leaked electrolyte and it is not good,
these welds are located right below the BMS wires solder pads and I remember having excess flux drip on the strips that I forgot to clean, so it is only residual flux and should be safe,
since I used superglue to fix the stainless steel pads before welding, it is an oily/burnt glue residue, so it should be safe but I'm not convinced by this one,
What do you think it is ?
What should I do to check ? Monitor the voltage of the corresponding p-groups ?
What is typical of cell puncturing in your experience ?
Thank you all again for your insight and have a nice day :)